Cathodic Protection of Pipe Encapsulated in Polyethylene Film

Case histories are presented where polyethylene encasement and cathodic protection have been used together to effectively control external corrosion of ductile iron pipelines in corrosive soils. The four case histories evaluated include impressed current and galvanic anode protection.