Hot Oil Aboveground Storage Tank Bottom Corrosion Failure and Cathodic Protection Upgrade—Part 2

Several types of anode installations for tank bottoms are possible, but the methods selected do not always produce the desired results. This two-part article discusses a case history in which existing cathodic protection (CP) was ineffective and testing methods did not identify system deficiencies. This led to the premature failure of the tank bottom. Part 1 covered the findings of an investigation conducted to identify the cause of the corrosion. Part 2 describes the remedial approach taken to enhance CP for effective corrosion control.