Restoration of a Brick Chimney with a Dual Lining System and Polymer Concrete

A brick flue at a generating station was in need of rehabilitation because of the spalling and cracking of the brick. This caused a leakage of acid gases into the annulus. A typical flash coat system was not desired because of its relatively short life. A system of corrosion-resistant materials, which has shown excellent performance and durability, was chosen to make the repairs. The system consists of a combination of organic and ceramic-based lining materials. A case history is presented, with descriptions of the operating environment and materials selection criteria.