Lead Contamination of Condensed Water

This article presents experimental data that show the solubility of lead in different waters. Specifically noted is the solubility of lead in condensed, or “pure,” water. It provides introductory information to those just entering the field of water corrosion and contamination as well as basic information to others not familiar with water corrosion and contamination.

  Download Article PDF