Check Solar Weather Before Performing Pipeline CP Evaluation
By STEPHEN R. JOHNSON on 5/27/2015 2:05 PM
After experiencing severe telluric current activity on
a pipeline, the author researched the subject. The
causes and effects of telluric currents are explained
and precautions for obtaining data on forecast
telluric activity are given.