Lining Prevents Biogenic Sulfide Corrosion In Wastewater Systems

Faced with serious concrete deterioration from biogenic sulfide corrosion within collection systems, engineers and municipalities are extending the service life of wastewater conveyance structures with the use of 100% solids polyamine systems designed for hydrogen sulfide (H2S) permeation resistance. This article explains how sewer interceptors, manholes, and lift stations were protected using fluid-applied linings.