Failure Analysis of a 30-in Subsea Oil Pipeline

This article presents the failure investigation of internal pitting corrosion on a 30-in (0.762-m) diameter subsea oil pipeline in western offshore India. Detailed laboratory and analytical studies were made on the failed sample to establish the cause and mechanism of failure. This article describes the analysis methodology, the probable corrosion and failure mechanism, and recommended preventive measures.

  Download Article PDF