Premium Connection Downhole Tubing Corrosion
By LU SHUANLU, XIANG JIANMIN, KANG YANJUN, CHANG ZELIANG, AND DONG XUNCHANG, AND ZHAI TONGGUANG on 5/27/2015 9:45 AM
This article discusses a field background search,
macro- and micro-corrosion morphology analysis,
and material testing of corroded premium
connection downhole tubing. Tubing failure was
caused by erosion-corrosion from highly disturbed
liquid and high shear stress at the couplings.