Corrosion Control Technologies for Wastewater Treatment Plants

Wastewater treatment plant components generally experience both atmospheric and immersion corrosion. Hydrogen sulfide (H2S), which is usually present, has wide-ranging effects in wastewater systems, most notably causing corrosion and odor problems. The corrosion problems can be mitigated by a combination of strategies including judicious selection and implementation of emerging corrosion-resistant coatings.