CIN (Maia, Portugal), a leading Portuguese brand in the Iberian paint and varnish market, has recently launched its new C-CRYL W680 MATT coating to fully protect concrete.
This new coating has a low level of volatile organic compounds (VOCs) is permeable to water vapor, has low permeability to carbon dioxide (CO2) and water, and displays good adhesion, according to the company.
This product is fire retardant and available in a wide range of colors, in unlimited amounts, and in the Colormix 3G fine tuning. It may be used directly on concrete or cement surfaces, or as a finish for water-based intumescent paints.
The 12-680 C-CRYL W680 MATT allows users to obtain a matte finish in protecting structural concrete and cementitious mortars for repair and finishing. Additionally, it displays good finish and opacity, even in roller applications.
The new water-based acrylic coating by CIN has the CE Marking by the European Commission (Brussels, Belgium), since it meets the requirements of Standard EN 1504-2. That means the product complies with the principles of protection against ingress, moisture control, and increasing resistivity.
CIN says the new product is a result of the company’s continuous investment in research and development (R&D) within the coatings market. The company notes that its products are also present in many international markets.