Study: North American Waterways Becoming Saltier, More Alkaline

University researchers find significant increases in both salinization and alkalinization of U.S. streams and rivers, which can influence the water's corrosivity.

Investigators Find Severe Corrosion in 2015 California Gas Leak

Independent investigators found extensive corrosion on the well casing that broke open at Southern California Gas Co.'s Aliso Canyon gas storage facility in October 2015. In the aftermath, engineering consultancy Blade Energy Partners was granted authority by the California Public Utilities Commission (CPUC) to conduct a root cause analysis of the metallurgical and fractographic aspects of the gas leak.

Geopolymer Solution for Sulfuric Acid Corrosion at Wastewater Plants

In a recently issued paper, Austrian researchers from TU Graz and the University of Graz discuss new materials that prevent damage from the microbiologically influenced corrosion of concrete.

Academic Study Seeks Policy Changes After Flint Water Crisis

University researchers issued findings on policy problems that led to the Flint water crisis and recommended legal changes to mitigate future concerns, including better communication on issues such as corrosion controls.

Test Samples of Reinforced Concrete Are Often Too Small

A recent study from European university scientists suggests that samples of reinforced concrete need to be larger to ensure accuracy in corrosion detection.

Roundtable on the Future of Corrosion Control: Part 2

Industry panelists share their predictions on where the corrosion industry is going in the next 25 years and beyond by predicting the corrosion control developments of the future. For Part 2 of this series, the featured panelist is Fred Goodwin, head of BASF Construction Chemicals Global Corrosion Competency Center.

Self-Healing Material Builds Itself from Carbon Exposure

The polymer, which might someday be used as construction or repair material or for protective coatings, continuously converts the greenhouse gas into a carbon-based material that reinforces itself, according to the researchers. This “self-healing material,” designed to mimic the absorption properties of green plants, has potential applications in a variety of construction and protective coatings projects.

New Sensing, Simulation Tools Predict Military Aircraft Corrosion

The Air Force Research Laboratory says it is developing a new environmental sensing platform and testing chamber apparatus to enable superior management of aircraft corrosion. Researchers are currently testing both devices, which they believe could help preemptively predict corrosive environmental conditions before they can cause damage to military assets.

Tank Integrity Studied at Radioactive U.S. Waste Storage Site

In the latest round of testing, investigators found that two tanks at the decommissioned Hanford nuclear production complex in Washington had spots showing significant thinning in a ring around the shell’s wall.

Underdeposit Corrosion in a Subsea Water Injection Pipeline

Underdeposit corrosion (UDC), a general term that refers to localized corrosion that develops beneath or around deposits on a metal surface, is a phenomenon that leads to pipeline failures and is one of the most damaging forms of corrosion for oil and gas pipelines. It can occur in subsea water injection pipelines, well-fluid pipelines, and large-diameter transmission lines.

Advanced Corrosion, Rust Drive Brake Pad Failures

A new study from the Global Brake Safety Council suggests the use of substandard materials and processes in automobile brake pads could be leading to accelerated failure modes. The council was formed in 2014 to advocate and raise awareness for high standards in brake safety while ensuring responsible manufacturing in the automotive industry.

Researchers Suggest New Method to Create Corrosion-Resistant Alloys

A new study suggests that a better protective oxide scale can be achieved in high-temperature Al alloys by controlling the size distribution of reactive element particles. These types of alloys are prevalent in many industrial sectors and applications.

The Humble Building Material that Shelters Millions Across the Globe

Corrugated iron has been and continues to be an invaluable building material that deserves to be taken seriously. It shows that steel can be simply and cheaply formed to a useful shape, protected from corrosion by a range of coatings, and made accessible to citizens in all corners of the globe.

Water Repellency Technology Mitigates Corrosion Under Insulation Risk

The hydrophobic WR-Tech additive leads to stone wool, mandrel-wound pipe sections with significantly less water absorption relative to industry standards; faster drying rates; and durability over a wide range of potential CUI temperatures.

Study: Microbial Corrosion Led to California Gas Leak

An investigative report into the 2015 blowout of a natural gas well near Los Angeles, California, USA, cited corroded pipe casings, safety failures by a utility, and inadequate regulations as incident causes.